When picking shows on food flexible packaging, what do you move first

When picking shows on food flexible packaging, drop viscosity and pressure first. Do not add ink. Change only this one thing. Look again in the same place after you change it. The solid edge lifts paper fiber and shows a white edge.

Picking on food flexible packaging

When picking shows on food flexible packaging, drop viscosity and pressure first. Do not add ink. Change only this one thing. Look again in the same place after you change it. The solid edge lifts paper fiber and shows a white edge.

Picking on food flexible packaging

Move one thing first

Stop if the sheet surface is torn. Light linting follows the sample. If it has already hit the ingredient list, an allergen line, or a barcode, stop first, then adjust. Do not try it while the press keeps running. A void is ink that never landed. The sheet surface is still whole.

Order

Do this first Do not do this first Why
Drop viscosity and pressure first. Do not add ink. Change ink, pressure, and speed at the same time Change three things at once and you will not know which one worked
It has already landed on the ingredient list, an allergen line, or a barcode Try it while the job keeps running Scrap keeps going
Log the paper batch, the viscosity, and the pressure. Only say you already adjusted it The next shift cannot pick it up

Leave this behind

  1. Drop viscosity and pressure first. Do not add ink.
  2. In the same place, confirm whether the picking has eased.
  3. Log the paper batch, the viscosity, and the pressure.